# 5160 or 80CrV2?

> Tests of 5160 and 80CrV2 side by side: toughness, hardenability, edge retention and the tempering limit each one has.

Source: https://knifetemplates.com/steel/5160-vs-80crv2

[Learn](https://knifetemplates.com/guides) / [Steel](https://knifetemplates.com/steel)

Both are low alloy steels forging bladesmiths use for working knives, so the question comes up whenever someone buys bar for a chopper or a camp knife. They were not tested head to head, which changes how to read the comparison.

[Knife Templates](https://knifetemplates.com/makers/knife-templates) · 3 min read

## They were tested separately

The 5160 study used Charpy specimens of 2.5 x 10 x 55 mm without any notch, and concluded that 5160 was better than any other steel tested apart from 8670. The 80CrV2 study found slightly better toughness than 1084. Those are different studies with different specimens and different heat treatments, so I do not put a number on which of the two is tougher.

Edge retention is the one place a source speaks about only one of them: the 80CrV2 testing puts its wear resistance, as measured by a CATRA edge retention test, very low on the chart. The 5160 article I use does not test edge retention, so I make no claim about it.

## The heat treatment is the real difference

5160 has a narrow best window: austenitizing at 1500 to 1525°F and tempering at 375 to 400°F gave the best combination of properties, with a Parks 50 oil quench followed by 15 minutes in liquid nitrogen. Tempering above 400°F or below 375°F is not recommended. 80CrV2 is more relaxed on the temper: the advice is not to temper it above 450°F, and a 300°F temper looks attractive for thin knives with high cutting performance.

Keep in mind where each route on this site comes from. The 80CrV2 route is the one from the independent tests. The 5160 route is a different one, from a supplier sheet, and the 5160 page explains why its numbers should not be mixed with the tested optimum.

*5160 and 80CrV2 compared*

|  | 5160 | 80CrV2 |
| --- | --- | --- |
| Stainless | No | No |
| Toughness | Better than any other steel tested apart from 8670, in Charpy tests | Slightly better toughness than 1084 |
| Edge retention | Not tested in the article used here | Wear resistance "very low on the chart" in CATRA testing |
| Austenitising in the tested route | 1500 to 1525°F in the best route | 1525°F for 10 minutes |
| Tempering in the tested route | 375 to 400°F, and not outside it | Not above 450°F; 300°F for thin knives |
| Quench in the route here | Medium-speed oil (Parks AAA) | Oil, fast or medium |

## Where this comes from

- [How to Heat Treat 5160: Optimizing Toughness](https://knifesteelnerds.com/2019/04/01/how-to-heat-treat-5160/), Knife Steel Nerds. Charpy tests of 5160 across austenitising and tempering temperatures, including a liquid nitrogen step. Its optimum belongs to that process.
- [How to Heat Treat 80CrV2](https://knifesteelnerds.com/2022/06/23/how-to-heat-treat-80crv2/), Knife Steel Nerds. Larrin Thomas’s tests of 80CrV2, with datasheet comparisons. Test coupons were sealed in stainless foil.
- [How to Heat Treat Knife Steel in a Forge](https://knifesteelnerds.com/2021/09/23/how-to-heat-treat-knife-steel-in-a-forge/), Knife Steel Nerds. A method for reducing forge error, tested on seven low alloy steels. The author still recommends a furnace or a professional for most people.
- [Knife Steels Rated by a Metallurgist: Toughness, Edge Retention, and Corrosion Resistance](https://knifesteelnerds.com/2021/10/19/knife-steels-rated-by-a-metallurgist-toughness-edge-retention-and-corrosion-resistance/), Knife Steel Nerds. One metallurgist’s ratings, which he says he may change. The rating tables are images, so this site quotes only the text.
- [5160 Heat Treat, July 2020](https://cdn.newjerseysteelbaron.com/wp-content/uploads/2020/07/5160-Heat-Treat-7-20.pdf), New Jersey Steel Baron. Supplier schedule for controlled equipment. Fahrenheit is authoritative where the PDF prints an inconsistent Celsius conversion. Example setpoints below sit inside its ranges; no hardness is guaranteed.
- [How to Heat Treat 80CrV2](https://knifesteelnerds.com/2022/06/23/how-to-heat-treat-80crv2/), Knife Steel Nerds. Original experiments by metallurgist Larrin Thomas. Starting microstructure, hold and quench stay together. Do not transfer experimental property values to a different process.

[Next up AEB-L or MagnaCut? Two stainless steels: composition, the properties each source reports, and what the routes ask of you.](https://knifetemplates.com/steel/aeb-l-vs-magnacut)

## Keep reading

- [Knife steel: 5160](https://knifetemplates.com/steel/5160)
- [Knife steel: 80CrV2](https://knifetemplates.com/steel/80crv2)
- [Knife steel: 8670](https://knifetemplates.com/steel/8670)
- [Which steel should your knife be?](https://knifetemplates.com/steel/which-steel)
- [Choosing steel for a knife](https://knifetemplates.com/steel)
- [All steel pages](https://knifetemplates.com/steel)

## Put it into practice

[Choose a template](https://knifetemplates.com/templates) [Read the print guide](https://knifetemplates.com/guides/print-at-actual-size) [Arrange blanks on stock](https://knifetemplates.com/nest)