# Knife steel: 52100

> What 52100 is, its toughness and hardenability from the tests, and why it is recommended over 1095 and O1.

Source: https://knifetemplates.com/steel/52100

[Learn](https://knifetemplates.com/guides) / [Steel](https://knifetemplates.com/steel)

52100 rewards a little attention to what happened before the final hardening heat. I would keep the whole process together here, including the anneal, rather than copy the last two temperatures from somebody's notes.

[Knife Templates](https://knifetemplates.com/makers/knife-templates) · 2 min read

## What it is

A non-stainless bearing steel used for fine cutting blades. The chromium in it does not make it stainless. Known bar makes the starting point clearer than an unidentified bearing race.

## What the testing found

52100 shows good toughness compared with other low alloy steels, and it has medium hardenability, so it straddles the line between water or fast oil and medium oil. The tested route is to austenitize at 1500-1525°F for 15 minutes and quench in fast oil, then temper between 300 and 400°F, the lower end for higher hardness and the higher end for better toughness.

The testing places it above its neighbours: 52100 over 1095 or O1 on toughness, and 52100 and CruForgeV are good for general purpose knives. In forge heat treating it is also the pick among the fine-cutting steels.

## Where to be careful

The tested process is not claimed to be the absolute best possible heat treatment. A cryo step can add about 0.5 Rc for applications that need maximum strength, at a small toughness cost. It is not stainless, so treat it like the other carbon steels and keep it dry.

## Where this comes from

- [How to Heat Treat 52100](https://knifesteelnerds.com/2019/05/13/how-to-heat-treat-52100/), Knife Steel Nerds. Larrin Thomas’s tests of 52100. The article says it makes no corrosion statements and does not claim to be the best possible treatment.
- [Bainite Heat Treatments of 52100, O1, and 1095: How Much Toughness?](https://knifesteelnerds.com/2021/06/07/bainite-heat-treatments-of-52100-o1-and-1095-how-much-toughness/), Knife Steel Nerds. Austempering experiments and what they say about plate martensite in 1095 and O1. A different route from quench and temper.
- [How to Pick the Best Steel for Every Knife](https://knifesteelnerds.com/2019/05/20/how-to-pick-the-best-steel-for-every-knife/), Knife Steel Nerds. Larrin Thomas’s method for choosing a steel, with his own recommendations. Opinion informed by his testing; the charts are images.
- [How to Heat Treat Knife Steel in a Forge](https://knifesteelnerds.com/2021/09/23/how-to-heat-treat-knife-steel-in-a-forge/), Knife Steel Nerds. A method for reducing forge error, tested on seven low alloy steels. The author still recommends a furnace or a professional for most people.
- [Knife Steels Rated by a Metallurgist: Toughness, Edge Retention, and Corrosion Resistance](https://knifesteelnerds.com/2021/10/19/knife-steels-rated-by-a-metallurgist-toughness-edge-retention-and-corrosion-resistance/), Knife Steel Nerds. One metallurgist’s ratings, which he says he may change. The rating tables are images, so this site quotes only the text.

[Next up Knife steel: O1 An oil-hardening tool steel that needs a long, controlled soak.](https://knifetemplates.com/steel/o1)

## Keep reading

- [Knife steel: 1095](https://knifetemplates.com/steel/1095)
- [Knife steel: 80CrV2](https://knifetemplates.com/steel/80crv2)
- [Choosing steel for a knife](https://knifetemplates.com/steel)
- [All steel pages](https://knifetemplates.com/steel)

## Put it into practice

[Choose a template](https://knifetemplates.com/templates) [Read the print guide](https://knifetemplates.com/guides/print-at-actual-size) [Arrange blanks on stock](https://knifetemplates.com/nest)