Learn / Heat treating

Heat treating 5160

5160 often comes up when makers talk about tough working blades. I would start with identified bar and a repeatable schedule rather than an unknown spring with years of service behind it.

Knife Templates · 4 min read

Where I would start

A non-stainless spring steel commonly considered for larger working knives. Thickness and edge geometry still decide much of how a finished blade cuts and survives use.

Annealed stock-removal material using the NJSB supplier route below. This is separate from the frequently quoted cryogenic toughness experiments on forged, normalised and annealed specimens.

Get the equipment ready

A controlled furnace, anti-scale protection, medium-speed commercial oil such as Parks AAA, and a verified tempering oven.

Measure the furnace and tempering oven independently where possible. A controller display is a setpoint, not proof that the whole blade has reached it. Timing a hold starts after equalisation, not as soon as the door closes.

A process to work from

Use this as a complete route to establish on a coupon from your stock. Temperatures in Celsius are rounded conversions of the Fahrenheit setpoints. A different supplier, section or starting condition can need a different process.

5160: worked heat-treatment route
StageWhat to do
AustenitiseExample: 802°C / 1475°F, inside the supplier’s 1465–1480°F window. Hold 10 minutes after equalisation, within its 5–15 minute allowance for section and equipment.
QuenchUse the supplier’s medium-speed oil route, for example Parks AAA, operated to the oil maker’s instructions.
TemperNear room temperature, begin 204°C / 400°F for 2 hours. Cool to room temperature and repeat for 2 hours.
Cold treatmentNone specified in this supplier route. Do not attach hardness or toughness figures from a cryogenic experiment to this process.

The detail to pay attention to

You will also find 1500–1525°F recommendations. Those can belong to a different tested process. Keep the prior treatment, oil, cold step and temper with the schedule they came from instead of taking the hottest number from each.

If using forged material, establish its normalising and annealing route before using a stock-removal schedule. If you cannot identify a recycled spring, treat it as an experimental material rather than stamp 5160 on the finished knife. Cracks from prior service are another uncertainty you do not need on an early build.

Check the result before fitting the handle

Clean scale and decarburisation from the test surface before interpreting a hardness reading. Use a flat, supported area and a calibrated method appropriate to the sample thickness. A file skating across a blade is a rough check, not an HRC measurement.

Inspect the tempered blade in good light for cracks, edge waves and distortion. If a blade is cracked, retire it. If hardness is unexpectedly low, check the whole record before increasing temperature or repeating a quench.

Keep a record

Keep the stock supplier and batch, blade and edge thickness, furnace program, actual hold, oil or plate details, cold-treatment branch and temper cycles beside the editable design. Add measured hardness and where it was measured.

After grinding and sharpening, evaluate the finished knife in its intended cutting work. Keep notes on edge stability, sharpening and geometry. Change one main variable so you can tell what helped as you learn.

Where this comes from

  • 5160 Heat Treat, July 2020, New Jersey Steel Baron. Supplier schedule for controlled equipment. Fahrenheit is authoritative where the PDF prints an inconsistent Celsius conversion. Example setpoints below sit inside its ranges; no hardness is guaranteed.
Next upHeat treating 5210052100: the equipment, hardening hold, quench, temper and details that are easy to miss.

Comments

Questions, corrections and what worked for you. Upvote comments you find useful.

Loading comments…

Knife Templates