What a spark test is
You touch the steel to a grinding wheel and read the sparks. Tharwa Valley Forge describes the patterns for several steels, and is clear about the limit: given the huge variety of steel, there are no guarantees.
| Steel | Sparks |
|---|---|
| Mild steel | White, with tiny forks and varied lengths. |
| Medium-carbon steel | More forking than mild steel, with a wide range of lengths. |
| High-carbon steel | A bushy pattern of forking that starts at the wheel, less bright than medium-carbon. |
| 300-series stainless | No forking, orange to straw. |
| Cast iron | Very short sparks that begin at the wheel. |
| Titanium | A brilliant, blinding white, though it is not a ferrous metal. |
Why it cannot name a steel
A pattern places a piece in a family (mild, medium carbon, high carbon, stainless). It does not tell you which alloy in the family, or what treatment it has had. An old spring may also have cracks from its service life. If you cannot identify a recycled spring, treat it as experimental material rather than stamping 5160 on the finished knife.
A quench test
Tharwa Valley Forge also suggests trying to harden a sample: "You can also try quenching in various ways to see if the sample can be hardened." That tells you whether the piece is useful, not what it is.
What I would do
Buy known bar with a grade, a supplied condition and a published schedule for a first knife. Keep experimental stock separate, label it as experimental, and make test knives from it that you do not sell as a named steel.
Where this comes from
- Recycled steel identification, Tharwa Valley Forge. Spark test descriptions for common steels. The page itself says there can be no guarantees given the variety of steel.
Comments
Questions, corrections and what worked for you. Upvote comments you find useful.